MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay MTM® 70
Categories: Polymer; Thermoset

Material Notes: Description: MTM70 is a toughened, variable cure temperature prepreg matrix formulated for the manufacture of structural components operating at elevated service temperatures. After 135°C (275°F) standard cure cycle. MTMT70 provides excellent mechanical performance for components operating at up to 140°C (284°F). After post-cure to 180°C (356°F), MTMT70 will operate at higher temperatures without significant loss of toughness.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage life at -18°C (0°F)
  • Initial cure temperatures between 85°C and 180°C (185°F to 356°F)
  • Tg steps ahead of cure temperature
  • Good mechanical performance with intermediate and high modulus fibers
  • Variable cure temperature capability
  • Excellent retention of mechanical properties at elevated temperatures
Note 1: Cure cycle: 1.5 hrs at 135°C (275°F), 6.2 bar (90 psi)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, Cured resin, 1.5 hrs at 135°C + 2 hr at 180°C
  • Storage Temperature
  • Compressive Strength, SRM 2R-94, T800 140-54%, After Impact, Post-cure: 2 hrs at 180°C, Note 1
  • Compressive Strength, SRM 2R-94, T800 140-54%, After Impact, Note 1
  • Compressive Strength, ASTM D3410, T800 140-54%, 0°, Note 1
  • Compressive Strength, ASTM D3410, T1000 140-54%, 0°, Note 1
  • Shear Strength, ASTM D2344, T1000 140-54%, 0°, Interlaminar, Note 1
  • Shear Strength, ASTM D2344, T800 140-54%, 0°, Interlaminar, Note 1
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1.5 hrs at 135°C
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1.5 hrs at 135°C + 2 hrs at 180°C
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.