Polyplate® P01 is a milled, high brightness, large particle size delaminated kaolin, intended for use in solvent and water-borne coatings, inks, and adhesives. The high aspect ratio of the large platy particles provides improved tinting strength, enamel holdout, and crack resistance. Industry: Paint & Coatings, Adhesives & Sealants, Rubber & Plastic Uses: Architectural Coatings, Industrial Coatings, Wood Coatings, Flat/Matte, Satin, Primer, Water Based, Solvent Borne, Non-Black Rubber Information provided by KaMin LLC. |