MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • High strength and toughness with excellent thermal stability to 400°F.
  • Outstanding chemical resistance.
  • Excellent electrical, and mechanical properties.
  • Ease of use.

Applications: Encapsule sensitive instrumentation for chemical isolation, outstanding moisture resistance, ruggedness and flexibility. Suitable for clean room use and direct contact with semiconductors. Very easy to use and very clean two-part system. Superior for coating in marine applications and other harsh environments. Tough, high strength, chemically resistant non-blush clear coating with medium gloss finish. Bonds to most substrates. Can be applied to oily surfaces. Ambient 24 hour or accelerated thermal cure.

Key Words: Epoxy Adhesive, Sealant
Vendors:
Available Properties
  • Water Absorption, 24hrs boiling DI water
  • Viscosity
  • Tensile Strength at Break, 3 hrs @ 200°F; 2:1 Volume Mix
  • Tensile Strength, Ultimate, Peak; 3 hrs @ 200°F; 2:1 Volume Mix
  • Tensile Strength, Yield, 3 hrs @ 200°F; 2:1 Volume Mix
  • Elongation at Break, 3 hrs @ 200°F; 2:1 Volume Mix
  • Elongation at Yield, 3 hrs @ 200°F; 2:1 Volume Mix
  • Tangent Modulus, 3 hrs @ 200°F; 2:1 Volume Mix
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Ambient Set
  • Cure Time, Ambient, 95% cure
  • Cure Time, 98% cure
  • Tack-Free Time, Ambient
  • Pot Life, Ambient
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Reltek LLC

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.