MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dongnam Realize CXP Flame Retardant Grade Cellulose Polymer
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: CXP stands for Cellulose X-linked Polymer, a polymer made by covalently bonded cellulose. Cellulose is the main component found in trees, it is present in various plants. CXP is a material that can be manufactured by replacing oxygen molecules in the main chain of the polymer, making it into a material that can be injected and extruded. It has the same basic characteristics of wood, but it is easier to process and manage. Compared to wood, it has a better durability, weather resistance, moisture resistance, and doesn't require any kind of lacquer or treatment. It uses forestry byproducts, so it can be produced at a low unit price while effectively utilizing discarded resources.

Information provided by Dongnam Realize.

Vendors:
Available Properties
  • Density, ASTM D256
  • Melt Flow, ASTM D1238
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Shrinkage, Manufacturer Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.