MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay BR® 680-3 Polyimide Film Adhesive
Categories: Polymer; Adhesive

Material Notes: Description: BR® 680-3 paste adhesive is a radar transparent, viscous/thixotropic material supplied at 60 – 65% solids. It is intended for bonding both metallic and non-metallic sandwich structures. It is equally suitable for bonding metals and composite laminates.BR 680-3 is co-curable at temperatures up to 700°F (371°C) with various polyimide composites. Although not mandatory, BR® 680 adhesive primer may be used to seal prepared metal surfaces.

Features & Benefits:

  • 700°F (371°C) service temperature
  • Developed specifically for honeycomb sandwich bonding
  • 350°F (177°C) processing
  • Radar transparent
  • Superior thermal oxidative stability
  • Co-curable with Avimid N and other poyimide composite materials
  • Condensation-type polyimide
Applications:
  • Honeycomb sandwich construction
  • Metal-to-metal bonding
  • Composite-to-metal bonding
  • Composite-to-composite bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Solids Content
  • Storage Temperature
  • Tensile Strength, Flatwise with 177°C cure cycle
  • Tensile Strength, Flatwise with 177°C cure cycle, with FM 680-1
  • Tensile Strength, Flatwise, metallic
  • Tensile Strength, Flatwise, non-metallic
  • Tensile Strength, Flatwise with 177°C cure cycle
  • Tensile Strength, Flatwise with 177°C cure cycle, with FM 680-1
  • Tensile Strength, Flatwise, metallic
  • Tensile Strength, Flatwise, non-metallic
  • Shear Strength, One-half Lap
  • Shear Strength, One-half Lap
  • Shear Strength, One-half Lap
  • Shear Strength, One-half Lap
  • Maximum Service Temperature, Air
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.