MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
UBE UBEPOL VCR® 450 Synthetic Polybutadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics: Broad molecular weight distribution type (Matrix BR). Good balanced between characteristics of VCR and the physical properties of general BR. Applications: Tires for passenger cars, trucks, buses, construction machinery, motorcycles and bicycles. Various industrial products such as polystyrene modifier, conveyor belts, hoses, rubber isolators and casters. Commodities such as shoe soles and golf balls.

UBEPOL VCR® consists of high-cis BR and high-crystalline syndiotactic polybutadiene resin which is a special type of polymer alloy. UBEPOL VCR® can contribute to produce various advantages: to increase hardness, modulus of rubber product without adding filler. To reduce the volume or weight of rubber product by utilizing its reinforcing effect. To improve extrusion properties (extrusion output and dimensional stability) and roll mill shrinkage.

Information provided by UBE Industries, LTD

Vendors:
Available Properties
  • Specific Gravity
  • Mooney Viscosity, ML1+4
  • Mooney Viscosity, Compound. ML1+4. ASTM D3189
  • Hardness, Shore A, Curing time: 50 min
  • Tensile Strength
  • Elongation at Break
  • 100% Modulus, Curing time: 50 min
  • 200% Modulus, Curing time: 50 min
  • 300% Modulus, Curing time: 50 min
  • Rebound, BS. Curing Time: 50 min
  • Tear Strength, Curing time: 50 min
  • Abrasion, Lambourn. Index. Slip rate 60%. Curing time: 50 min
  • Abrasion, Lambourn. Index. Slip rate 20%. Curing time: 50 min
  • Abrasion, Pico. Index. Curing time: 50min
  • Compression Set, Curing time: 50 min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.