Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings. Forms Available: Lump or powder (100 mesh x down, 250 mesh by down or 400 mesh by down)Information provided by Reade Advanced Materials. |
CaMg(CO3)2 and CaMg(SiO3)2, Calcium-magnesium silicate, calcium-magnesium pyroxene, malacolite, alalite |