MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemours Teflon® FEP CJ-95 Fluoropolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: DuPont™ Teflon® FEP CJ-95 is a melt-processible fluoropolymer resin specifically designed for cable insulation and jacketing applications that demand a high degree of stress crack resistance.

This resin provides the electrical and mechanical properties needed for low-voltage applications. Teflon® FEP CJ-95 has a higher melt flow rate than Teflon® FEP 140, but it retains similar stress crack resistance.

Like all Teflon® fluoropolymer resins, Teflon® FEP CJ-95 offers an excellent combination of properties: chemical inertness, exceptional dielectric properties, heat resistance, toughness, flexibility, low coefficient of friction, nonstick characteristics, negligible moisture absorption, low flammability, performance at temperature extremes, and weather resistance.

Teflon® FEP CJ-95 can be processed by conventional thermoplastic techniques, melt extrusion and transfer molding. It shows, compared to Teflon®FEP 140, a higher MFR and critical shear rate at processing temperatures. In similar constructions, it can be processed at much higher rates and line speeds. The final product will show comparable physical properties. It can be used in place of Teflon® FEP 100 when the application requires a higher degree of stress crack resistance.

Stress crack resistance is an important element in establishing end-use performance. Extensive testing of wire and cable constructions is required for definitive performance evaluation. However, the MIT folding endurance or flex life test (ASTM D2176), when performed on a thin film of resin, can have a good correlation with extensive cable testing. The higher the MIT flex life, the higher the stress crack resistance of the resin. The folding endurance of the high productivity grade Teflon® FEP CJ-95 is marginally inferior to Teflon® FEP 140. DuPont does, however, always recommend, in particular for applications involving repeated thermal and flex cycling, to undertake more extensive and more specific tests on the final product itself. The MIT test results should be viewed as a guide to comparative performance of the various grades of resin.

Applications

Teflon® FEP CJ-95 fluoropolymer resin is used in many applications. One of the largest uses is as a jacket for telecommunications/data cables where Teflon® FEP CJ-95 not only provides excellent fire performance and physical properties but also superior electrical performance. In this role, it is ideal as a jacket material for constructions meeting Article 725 and Article 800 of the National Electric Code (NEC) where Teflon® FEP CJ-95 provides superior dielectric properties for rapid, clear signal transmission. Because of its exceptionally low flame and smoke properties, cables made with Teflon® FEP CJ-95 can be made to meet the requirements of Underwriters Laboratory “UL 910 Steiner Tunnel Test” for installation in plenums without metal conduits.

As a cable jacket, Teflon® FEP CJ-95 helps ensure long, reliable cable life and easy, economical installation. Its low coefficient of friction and flexibility makes cables easy to pull around corners and obstacles and through air-return plenums. Its toughness and abrasion resistance help eliminate cut-through and other damage that can occur during installation. Because jacketing of Teflon® FEP minimizes reel set, it provides for fast, economical installation. Cables jacketed with Teflon® FEP possess the outstanding chemical resistance of Teflon® FEP and stand up to most exposure conditions, including: heat, weather, ultraviolet light, and moisture.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors:
Available Properties
  • Specific Gravity, ASTM D762
  • Water Absorption, ASTM D570, 24 hours
  • Melt Flow, ASTM D2116
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D1708
  • Elongation at Break, ASTM D1708
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D1531
  • Dielectric Strength, ASTM D149, 10 mil film
  • Dissipation Factor, ASTM D1531
  • Arc Resistance, ASTM D495
  • Melting Point, ASTM D2116
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Processing Temperature, Cure Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.