MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
EDRO #2 Prehardened 4130 Holder Block
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Chrome-moly Steel

Material Notes: EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition.
EDRO #2™ is characterized by excellent machinability, good resistance to indentation, and uniform hardness in all dimensions.
Applications: holders/bolsters for plastic molds and die-casting dies, plastics and rubber molds with low requirements on polishability, support plates, and constructional parts

Information provided by EDRO

Key Words: AISI 4130-35 improved
Vendors:
Available Properties
  • Hardness, Brinell
  • Hardness, Vickers, Nitriding in ammonia gas
  • Hardness, Vickers, Tufftriding (Tenifer process)
  • Tensile Strength, Ultimate, Round bar 1" diameter, 310 HB
  • Tensile Strength, Ultimate, Round bar 1" diameter, 310 HB
  • Tensile Strength, Ultimate, Round bar 1" diameter, 310 HB
  • Tensile Strength, Yield, Round bar 1" diameter, 310 HB
  • Tensile Strength, Yield, Round bar 1" diameter, 310 HB
  • Tensile Strength, Yield, Round bar 1" diameter, 310 HB
  • Elongation at Yield, in 2"
  • Elongation at Yield, in 2"
  • Elongation at Yield, in 2"
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Charpy Impact, Round bar 1" diameter, 310 HB
  • Charpy Impact, Round bar 1" diameter, 310 HB
  • Charpy Impact, Round bar 1" diameter, 310 HB
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.