MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent filler acceptance makes Elvaloy® 1126 AC suitable for highly filled compounds.

Elvaloy® 1126 AC is easily processed on standard equipment used for low-density polyethylene.

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors:
Available Properties
  • Density, ASTM D792 - ISO 1183
  • Melt Flow, ASTM D1238 - ISO 1133
  • Hardness, Shore A, ASTM D2240 - ISO 868
  • Hardness, Shore D, ASTM D2240 - ISO 868
  • Tensile Strength at Break, ASTM D638 - ISO 527-2, 500 mm/min
  • Elongation at Break, ASTM D638 - ISO 527-2, 500 mm/min
  • Tensile Modulus, ASTM D638 - ISO 527-2, 1 mm/min
  • Melting Point, ASTM D3418 - ISO 3146, By DSC
  • Vicat Softening Point, ASTM D1525 - ISO 306, A50 (10N)
  • Processing Temperature, For blow molding
  • Rear Barrel Temperature, Extrusion lamination and extrusion coating
  • Rear Barrel Temperature, Cast film
  • Rear Barrel Temperature, Blown film
  • Middle Barrel Temperature, Blown film
  • Middle Barrel Temperature, Cast film
  • Middle Barrel Temperature, Extrusion lamination
  • Front Barrel Temperature, Blown film
  • Front Barrel Temperature, Cast film
  • Front Barrel Temperature, Extrusion lamination
  • Adapter Temperature, Blown film
  • Adapter Temperature, Cast Film
  • Adapter Temperature, Extrusion lamination
  • Die Temperature, Blown film
  • Die Temperature, Cast film
  • Die Temperature, Extrusion lamination
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Packaging and Industrial Polymers

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.