MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chevron Phillips Marlex® H516 Polyethylene; HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: High density polyethylene compound. This high performance PE 100 HDPE compound is tailored for the demanding requirements of pressure pipe applications that require:
  • Excellent long-term hoop strength
  • Superb resistance to slow-crack growth
  • Exceptional resistance to rapid-crack propagation
  • Outstanding low-temperature toughness
Additional information: Yellow version also available.

Applications: Typical pipe applications for H516 include:

  • Gas distribution
  • Potable water
  • Industrial applications

Information provided by Phillips

This compound meets or exceeds:

  • ASTM D4976 - PE 235
  • ASTM D3350, class 445574C and 445576C
  • NSF Standards 14 and 61 for potable water
  • PPI designations PE 4710 and PE 100
Vendors:
Available Properties
  • Density, ASTM D-1505
  • Melt Flow, ASTM D-1238, HLMI, 190/21.6
  • PENT, ASTM F-1473, slow crack growth
  • Tensile Strength, Yield, ASTM D-638, 2 in/min, Type IV bar
  • Elongation at Break, ASTM D-638, 2 in/min, Type IV bar
  • Flexural Modulus, ASTM D-790, Secant; 16:1 span:depth, 0.5 in/min
  • Hydrostatic Design Basis, ASTM D-2837
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chevron Phillips Chemical Company LP; ChevronPhillips

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.