MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used as bushings, rollers, wear strips and other applications requiring a combination of strength, low moisture absorption, chemical resistance, and dimensional stability.

Features:

  • No centerline porosity
  • Low moisture absorption
  • excellent machinability
  • Good combination of mechanical properties
  • Resistance to food industry cleaning chemicals, including aqueous solutions with pH between 4 and 14
  • Good wear and abrasion properties
  • Manufactured from resin and color components that are FDA, USDA, and 3A Dairy compliant
  • Good dimensional stability
  • Good property retention at elevated temperatures

    Information supplied by Ensinger, Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570, 24 hrs
  • Water Absorption at Saturation, ASTM D570
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, Dynamic, ASTM D3702, 40 psi, 50 fpm
  • K (wear) Factor, ASTM D3702, vs steel; 40 psi, 50 fpm
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150, 50% RH
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Melting Point, ASTM D2133
  • Maximum Service Temperature, Air, UL 746B, Long Term
  • Maximum Service Temperature, Air, Intermittent
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • USDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.