GY-TM-182 is a revolutionary high-performance stabilizer processing by polyvinyl chloride (PVC), its stability? transparency?weather resistance and low toxicity are superior to other traditional organic tin products. Advantages: - High value-added: GY-TM-182 is a revolutionary highperformance stabilizer processing by polyvinyl chloride (PVC), its stability?transparency? weather resistance and low toxicity are superior to other traditional organic tin products.
- Excellent transparency: GY-TM-182 provides excellent transparency to PVC products. European?United States and Japan manufactures have widely used GY-TM-182 in PVC colored?transparent and high transparent products.
- Extensive processing: With excellent color stability in high temperature and long-term dynamic stability, no scaling phenomenon, reduce the cleaning time of equipment. It can widely use in various machining processes of soft and hard polyvinyl chloride (PVC), such as rolling? extrusion?injection molding and blow molding related products.
- Volume of use: The dosage of GY-TM-182 is less than the traditional toxic butyl tin, octyl tin under the same thermal stability condition. Efficiency, and it can reduce costs.
- Excellent stability: GY-TM-182 has high thermal stability and excellent initial tinting ability.
- Nontoxic: GY-TM-182 products have already replaced toxic butyl tin and octyl tin products which are eliminated from the world and European Union. They can widely use in food packaging materials, PVC pipe materials and wide range of PVC products; safety and reliable.
Applications: - High-value PVC colorful products, partial and high transparency products
- GY-TM-182 can completely replace the traditional lowvalue and toxic butyl tin, octyl tin stabilizers.
- PVC particles (masterbatch, pellets, electronic communication equipmentsetc. )
- PVC building materials (plastic doors and windows, water pipes, pipe fittings, chemical pipes, building materials, shaped extrusion materials etc.)
- Medical devices,a variety of food package materials, household appliances and other PVC products.
- PVC sheets (Transparent soft and hard films, Christmas films, advertising films, composite films, etc.)
- PVC film (shrink packing film, printing film, rolling film, kink film)
- PVC rigid, semi-soft cloth, rubber products and PVC synthetic leather
- PU synthetic resin, foam processing applications, polyurethane resin synthesizes catalyst
Information provided by Go Yen Chemical |