MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Hexcel® HexPEKK® 100 for LPBF Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Description: HexPEKK®-100 is an electrostatic dissipative material developed for additive manufacturing with laser powder bed fusion (LPBF) technology. HexPEKK®-100 is highly chemically resistant and low-outgassing, with a wide service temperature range. Compliance to FAR 25.853 flammability, smoke and toxicity puts HexPEKK®-100 at the core of aerospace requirements and parts are currently in use for commercial aviation, crewed space, satellite, military aviation, and defense applications. Combining the flexibility of laser powder bed fusion technology with an engineering grade material 50% lighter than aluminum, HexPEKK®-100 is the perfect solution for your aerospace needs.

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Density, ASTM D792
  • Tensile Strength, ETW, Z
  • Tensile Strength, ETW, X
  • Tensile Strength, ETW, Z
  • Tensile Strength, ETW, X
  • Tensile Strength, ETW, Z
  • Tensile Strength, RTA, Z
  • Tensile Strength, CTD, Z
  • Tensile Strength, CTD, Z
  • Tensile Strength, ETW, X
  • Tensile Strength, CTD, X
  • Tensile Strength, RTA, X
  • Tensile Strength, CTD, X
  • Elongation at Break, CTD, Z
  • Elongation at Break, CTD, X
  • Elongation at Break, CTD, Z
  • Elongation at Break, RTA, Z
  • Elongation at Break, CTD, X
  • Elongation at Break, ETW, Z
  • Elongation at Break, RTA, X
  • Elongation at Break, ETW, X
  • Elongation at Break, ETW, Z
  • Elongation at Break, ETW, X
  • Elongation at Break, ETW, Z
  • Elongation at Break, ETW, X
  • Tensile Modulus, ETW, Z
  • Tensile Modulus, ETW, X
  • Tensile Modulus, ETW, Z
  • Tensile Modulus, ETW, Z
  • Tensile Modulus, RTA, Z
  • Tensile Modulus, CTD, Z
  • Tensile Modulus, ETW, X
  • Tensile Modulus, ETW, X
  • Tensile Modulus, RTA, X
  • Tensile Modulus, CTD, Z
  • Tensile Modulus, CTD, X
  • Tensile Modulus, CTD, X
  • Flexural Strength, ASTM D790, Z, 4-point
  • Flexural Strength, ASTM D790, X, 4-point
  • Flexural Modulus, ASTM D790, Z, 4-point
  • Flexural Modulus, ASTM D790, X, 4-point
  • Flexural Strain at Break, ASTM D790, Z, 4-point
  • Flexural Strain at Break, ASTM D790, X, 4-point
  • Compressive Strength, ASTM D695, Z, 2% Offset Yield
  • Compressive Strength, ASTM D695, X, 2% Offset Yield
  • Compressive Modulus, ASTM D695, Z
  • Compressive Modulus, ASTM D695, X
  • Poissons Ratio, ASTM D638, Z
  • Poissons Ratio, ASTM D638, X
  • Volume Resistivity, ASTM D257
  • CTE, linear, ASTM E831
  • CTE, linear, ASTM E831
  • Thermal Conductivity, ASTM D7984, X
  • Thermal Conductivity, ASTM D7984, X
  • Thermal Conductivity, ASTM D7984, Z
  • Thermal Conductivity, ASTM D7984, Z
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM D3418
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.