MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Foral™ AX-E Fully Hydrogenated Rosin
Categories: Other Engineering Material

Material Notes: Product Description: Foral™ AX-E Fully Hydrogenated Rosin is a thermoplastic, acidic resin produced by hydrogenating rosin to an exceptionally high degree. It is the palest, most highly stabilized rosin commercially available. Compared with Staybelite™ Resin-E Partially Hydrogenated Rosin, a hydrogenated rosin long established and widely used for its pale color and high oxidation resistance, Foral™ AX-E Fully Hydrogenated Rosin has better initial color and color retention, and even greater resistance to oxidation. It is especially indicated as the tackifier and resin modifier in solvent adhesives and hotmelt applied coatings and adhesives that must excel in these properties.

Application/Uses:

  • Assembly
  • Bookbinding
  • Caulks and Sealants
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Packaging
  • Paint and Coatings
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
  • Waterborne Adhesives
  • Wax Modification
Key Attributes:
  • Alcohol-soluble
  • Excellent resistance to oxidation
  • Medium softening point
  • Thermoplastic hydrogenated resin
  • Very light color

Information provided by Eastman

Vendors:
Available Properties
  • Total Acid Number, [mg KOH/g]
  • Softening Point, Hercules drop method
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.