BMC RF 9/35 is a bulk molding compound based on an unsaturated polyester resin, fire retardant grade, halogen-free, reinforced with glass fibers. This BMC has been developed for electrical application. Excellent mechanical properties and good fire protection grade are combined into the BMC RF 9/35 . BMC RF 9/35 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |