Peroxide cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Complies with FDA code of Federal regulations title CFR21 section 177.2600. Water and n-hexane tested. Also complies to the requirements of USP 25, NF20, 2002, Class 6. To meet ASTM D2000/SAE J200 line call-out M3CA507, A25, B35, EA14, F17. Applications: Excellent water and steam resistance with good compression set properties. Heat and chemical resistance is superior to that of sulphur cured EPDM. Not oil resistant. |