Product Description: Akroform S-80/EPR/P is an 80% polymeric dispersion of sulfur in EPR. The product is in the form of soft, ¼ inch cylindrical pellets. The soft pellets create an easy-to-weigh and easy-to-disperse quality sulfur masterbatch for applications that required exceptional sulfur dispersion. Advantages: Polymer bound or encapsulated dispersions are a proven means of upgrading plant safety, efficiency, quality & raw material control. Akrochem polymer bound or encapsulated chemical dispersions eliminate any irritating dust, as well as other potential hazards in handling powders in the plant. The physical form is easy to handle and weigh accurately. With a dispersion, better uniformity of the mix at lower processing temperatures is possible. Information provided by Akrochem Corporation |