MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Angst+Pfister APSOplast® UP GM 203-1 UP GM Hm 2471
Categories: Polymer; Thermoset

Material Notes: (polyester resin glass filament mat)

General description: In cases where laminated paper is not strong enough but the top values of laminated glass fabric are not required, polyester resin laminated glass mat makes for an inexpensive alternative. This grade impresses users with its high mechanical strength and top electrical insulation. As well as complying with the most import ant standards, polyester resin laminated mats are suitable for further requirements. Due to the good electrical properties of this grade, it is used successfully in the electrical industry. Winding supports for dry transformers, partitions, switch levers in high-voltage switches, and insulators for choke coils – just some of the numerous poss ible uses.

Characteristics and properties:

  • High dimensional stability
  • Very good dielectric properties
  • High temperature resistance, temperature limit of +155 °C as per VDE (Heat Insulation Class F)
  • Self-extinguishing, meets the requirements of UL94 V-0 from 2.4 mm (type GPO-3)
  • High track and arc resistance (type GPO-3)

Information provided by Angst + Pfister

Vendors:
Available Properties
  • Density, ISO 1183
  • Tensile Strength, ISO 527
  • Modulus of Elasticity, ISO 178, flexural test
  • Flexural Strength, ISO 178
  • Compressive Strength, ISO 604, resistance, perpendicular to layers
  • Charpy Impact Unnotched, ISO 179/3C
  • Dielectric Strength, IEC 60243-1, at 90°C in oil parallel to layers
  • Dielectric Loss Index, DIN 53483, after 24 h immersed in water
  • Comparative Tracking Index, IEC 60243-1, [kV], at 90°C in oil parallel to layers
  • CTE, linear, VDE 0304/2
  • Thermal Conductivity, DIN 52612
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.