MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay BR® 4535A Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: BR® 4535A is a single component, 100% solids, aluminum filled, epoxy adhesive. It has been developed for structural bonding and applications requiring increased adhesive flexibility and impact resistance with structural service performance to 150°C (302°F). Moderate temperature cure and good shelf stability give wide application to most manufacturing locations

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density
  • Solids Content
  • Storage Temperature
  • Tensile Modulus, Young's, Cure Cycle: 30 minutes at 150°C (300°F)
  • Shear Modulus, Cure Cycle: 30 minutes at 120°C (250°F)
  • Shear Modulus, Cure Cycle: 30 minutes at 150°C (300°F)
  • Shear Strength, 12 months, Long term Salt Spray
  • Shear Strength, Lap, 14 days 100% RH at 37°C (100°F)
  • Shear Strength, Lap, 30 days Oven aging at 71°C (160°F)
  • Shear Strength, 18 months, Long term Salt Spray
  • Shear Strength, Initial, Long term Salt Spray
  • Shear Strength, Lap, 30 days Salt spray
  • Shear Strength, 4 months, Long term Salt Spray
  • Shear Strength, 8 months, Long term Salt Spray
  • Shear Strength, Lap, 30 days Water immersion at 25°C (77°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 120°C (250°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 120°C (250°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 135°C (275°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 150°C (300°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 135°C (275°F)
  • Shear Strength, ASTM D1002, Lap, 60 min. at 120°C (250°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 120°C (250°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 150°C (300°F)
  • Shear Strength, ASTM D1002, Lap, 60 min. at 120°C (250°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 135°C (275°F)
  • Shear Strength, ASTM D1002, Lap, 30 min. at 150°C (300°F)
  • Shear Strength, ASTM D1002, Lap, 60 min. at 120°C (250°F)
  • Impact Test, 30 days Salt spray
  • Impact Test, 14 days Water immersion at 54°C (130°F)
  • Impact Test, 30 days 100% RH at 37°C (100°F)
  • Impact Test, 30 days Water immersion at 25°C (77°F)
  • Impact Test, 30 days Oven aging at 71°C (160°F)
  • Impact Test, ASTM D950
  • Impact Test, ASTM D950
  • Impact Test, ASTM D950
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, Cure Cycle: 30 minutes at 150°C (300°F)
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.