MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tra-Con Tra-Bond K5NA Ablative Thermal Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND K5NA is a three-part, ablative and thermally insulating epoxy compound used in aerospace applications. This smooth, trowellable system is specified by NASA for the Space Shuttle`s solid rocket boosters for close-out and patching of the boosters` thermal protection systems. It is also used for void filling and protecting wires, tubing and other surface protrusions on hypersonic re-entry bodies, nose cones and aircraft engines. TRA-BOND K5NA is impact resistant which makes it an excellent choice for lightweight casting requirements. TRA-BOND K5NA develops strong bonds to most all substrates. It maintains excellent dimensional stability over a wide temperature range and provides protection to weathering, ozone and moisture.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Solids Content, Reactive Solids Content
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Izod Impact, Notched
  • Thermal Conductivity
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.