MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Sandvik APM 2730 Hot Isostatic Pressed (HIP) Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: APM 2730 is a high alloyed powder metallurgical high speed steel corresponding to ASTM M3:2 +Co with a combination of very good abrasive wear resistance, high compressive strength and good high temperature properties. Suitable areas of use include demanding cold-work applications like blanking of harder materials like carbon steel or cold-rolled strip steel, as well as use for cutting tools. As with all powder metallurgy tool steels, machinability and grindability are superior to conventional high speed steel due to the very fine microstructure. Thanks to the fully homogenous material achieved in the powder metallurgy process, the dimensional stability after heat treatment is excellent. The process also ensures that the cleanliness of the steel is very high with a low amount of non-metallic inclusions. Compared to APM 2723 it has higher compressive strength and increased high temperature properties.

Information provided by Sandvik

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C, tempering temperature 600°C
  • Hardness, Rockwell C, tempering temperature 600°C
  • Hardness, Rockwell C, tempering temperature 600°C
  • Hardness, Rockwell C, tempering temperature 560°C
  • Hardness, Rockwell C, tempering temperature 520°C
  • Hardness, Rockwell C, tempering temperature 600°C
  • Hardness, Rockwell C, tempering temperature 560°C
  • Hardness, Rockwell C, tempering temperature 520°C
  • Hardness, Rockwell C, tempering temperature 600°C
  • Hardness, Rockwell C, tempering temperature 560°C
  • Hardness, Rockwell C, tempering temperature 520°C
  • Hardness, Rockwell C, tempering temperature 560°C
  • Hardness, Rockwell C, tempering temperature 560°C
  • Hardness, Rockwell C, tempering temperature 520°C
  • Hardness, Rockwell C, tempering temperature 520°C
  • Modulus of Elasticity
  • CTE, linear
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Molybdenum, Mo
  • Tungsten, W
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.