MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Elastron® V TPV Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Characteristics
  • wide hardness range
  • does not require vulcanisation-quite higher saving on the processing costs
  • remains flexible at low temperatures
  • high temperature resistance
  • electrical insulator with very low conductivity
  • has grades with very low conductivity
  • has grades with very low compression set
  • grades with very high abrasion resistance
  • excellent tear resistance
  • 100% recyclable
  • PVC free
  • resistance to solvents
  • resistance to oil
  • resistance to acids, bases, and detergents
  • resistance to UV and ozone
  • resistance to bacterial and fungus growth
  • has low toxic potential, with many grades conforming with FDA regulations
  • halogen free flame retardancy
  • coloured grades available
  • allows direct colouring during processing by utilizing coloured PP and PE masterbatches
  • 2-shot moulding onto many other plastics
  • appropriate co-extrusion process

Vendors:
Available Properties
  • Density
  • Hardness, Shore A
  • Hardness, Shore D
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Shrinkage
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.