MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Goodfellow Reaction Bonded Silicon Nitride Si3N4
Categories: Ceramic; Nitride

Material Notes: Reaction Bonded Silicon Nitride is produced by nitriding compacted Silicon powder. This production route is considerably more cost-effective than hot-pressing. Very complex and accurate shapes can be produced, which hold their shape during firing. After firing, as for Hot Pressed Silicon Nitride, it can be diamond ground to tolerances as close as 0.01mm. Although not as strong as Hot Pressed Silicon Nitride, its strength is held up to 1400°C, with long term oxidation resistance up to 1150°C. The thermal and electrical properties of the two forms of Silicon Nitride are very similar. RBSN finds use as supports in situations of continuous temperature cycling within ranges of up to 1000°C, as well as for gas turbine components. Reaction Bonded Silicon Nitride is resistant to a wide range of chemicals and molten metals. Silicon Nitride spheres have found use as bearings in the automotive industry, as they have high wear resistance and have a coefficient of friction and a density much lower than steel.

Information provided by Goodfellow.

Key Words: Si3N4; RBSN, NITRASIL® R
Vendors:
Available Properties
  • Density
  • Porosity, Apparent
  • Hardness, Vickers, kgf/mm²
  • Tensile Modulus
  • Compressive Strength
  • Shear Strength
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, long term
  • Maximum Service Temperature, Inert, continuous
  • Si3N4
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.