MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Poco Graphite Premium Silicon Carbide SUPERSiC® Silicon Carbide SUPERSiC®-H
Categories: Ceramic; Carbide

Material Notes: SUPERSiC is a silicon carbide material created and customized precisely for specific applications. SUPERSiC® Silicon Carbide Ideal for industrial, photovoltaic, semiconductor and aerospace optics application. SUPERSiC®-H is the base converted silicon carbide with extra processing to reduce non-metallic impurities. This material is ideal for high-temperature and atmospheric processes and harsh process environments. Features: Ultra high pure material with very low metallic contamination (less than 1 ppm total). Unique conversion process produces high quality silicon carbide. Superb resistance to chemical, thermal, and process erosion. Near-net shaping process allows for complex shapes with reduced post machining. Improved cost of ownership vs competitive materials. Applications: Plasma etch. RTP applications.

Information provided by Entegris POCO Materials.

Vendors:
Available Properties
  • Bulk Density
  • Apparent Bulk Density
  • Open Porosity
  • Porosity, Total
  • Hardness, Knoop, kg/mm2
  • Tensile Strength
  • Modulus of Elasticity
  • Flexural Strength
  • Poissons Ratio
  • Fracture Toughness
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear, @ RT
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Poco Graphite - Entegris

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.