MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Magnesium EQ-21A-T6, Sand/Permanent Mold Castings
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Typically used for commercial and military sand and permanent-mold castings used in the solution-treated and artificially aged condition (T6 temper) with high yield strengths up to 200°C. Alloy is equivalent to QE22A, but with lower silver content, and thus lower cost. Castings have excellent short-time elevated-temperature mechanical properties and are pressure tight and weldable.

Key Words: UNS M18330; European EN 1753 MC65220; AMS 4417; ASTM B 80; ASTM B 199; ASTM B 403 (Ingot UNS M18330)
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, 500 kg load, 10 mm ball
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Tensile Modulus
  • Compressive Yield Strength
  • Compressive Strength
  • Poissons Ratio
  • Fatigue Strength, Rotating Beam, R=-1, Notched, Kt=2
  • Fatigue Strength, Rotating Beam, R=-1, Notched, Kt=2
  • Fatigue Strength, Unnotched, Rotating Beam, R=-1
  • Fatigue Strength, Unnotched, Rotating Beam, R=-1
  • Fatigue Strength, Unnotched, Rotating Beam, R=-1
  • Fatigue Strength, Unnotched, Rotating Beam, R=-1
  • Shear Modulus
  • Electrical Resistivity
  • Heat of Fusion
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Casting Temperature, Sand Casting
  • Copper, Cu
  • Magnesium, Mg, As Remainder
  • Neodymium, Nd, Nd-rich rare earths
  • Nickel, Ni
  • Other, total
  • Silver, Ag
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.