MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay CYCOM® 977-20 Resin System with PRIFORM™ Technology  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: CYCOM® 977-20 RTM with PRIFORM™ Technology is a 177°C (350°F) curing toughened liquid epoxy resin system. CYCOM 977-20 RTM with PRIFORM Technology is formulated as the RTM version of Cytec Engineered Materials’ established CYCOM® 977-2 toughened epoxy prepreg resin. CYCOM 977-2 is widely used in many aerospace applications including primary and secondary aircraft structures, space and ballistics structures or any application requiring excellent impact resistance. CYCOM 977-20 RTM resin has a low viscosity to allow injection at temperatures between 60°C and 85°C (140°F and 185°F) without the need for excessive heating of resin transfer pipe work or high injection pressures. After injection, the resin viscosity decreases to below 50 cP, thus helping to ensure full fiber wetting. CYCOM 977-20 RTM resin is fully cured following a three-hour dwell at 177°C (350°F) after which it has a service temperature of 135°C (275°F). CYCOM 977-20 RTM resin must be used in conjunction with Cytec Engineered Materials’ patented PRIFORM hybrid fabrics in order to achieve cured performance properties equivalent to CYCOM 977-2 prepreg materials. The unique self-binding aspect of PRIFORM reinforcements removes the need for ancillary binder products and allows the manufacture of high quality preforms. The level of self-binding can be tailored from lightly stabilized, to aid cutting and handling of single plies, to highly compacted for high fiber volume preform construction.

Features & Benefits:

  • One part system; liquid at room temperature
  • RTM version of CYCOM 977-2 prepreg resin; suitable for primary aircraft structure
  • Excellent compression strength
  • Excellent compression strength after impact
  • Highest FST properties of all structural epoxy based composites
  • Injectable at 60°C to 85°C (140°F to 185°F)
  • Less than 200 cP initial injection viscosity
  • Minimum viscosity < 50 cP
  • 177°C (350°F) cure giving service temperature of 135°C (275°F)
  • Shelf life of 12 months at -18°C (0°F) and out life of 30 days at 22°C (72°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Tensile Strength, 6K HTA 5HS 370 gms
  • Tensile Strength, 6K HTA 5HS 370 gms
  • Tensile Strength, wet, 6K HTA 5HS 370 gms
  • Tensile Strength, 24K IMS WNCF 550 gsm
  • Tensile Strength, wet, 24K IMS WNCF 550 gsm
  • Tensile Strength, 24K IMS UW 200 gsm
  • Tensile Modulus, 6K HTA 5HS 370 gms
  • Tensile Modulus, wet, 6K HTA 5HS 370 gms
  • Tensile Modulus, wet, 24K IMS WNCF 550 gsm
  • Tensile Modulus, 24K IMS WNCF 550 gsm
  • Tensile Modulus, 24K IMS UW 200 gsm
  • Compressive Strength, After 25J Impact, 24K IMS WNCF 550 gsm
  • Compressive Strength, Open Hole, wet, 6K HTA 5HS 370 gms
  • Compressive Strength, After 25J Impact, 6K HTA 5HS 370 gms
  • Compressive Strength, Open Hole, wet, 24K IMS WNCF 550 gsm
  • Compressive Strength, Open Hole, 6K HTA 5HS 370 gms
  • Compressive Strength, Open Hole, 24K IMS WNCF 550 gsm
  • Compressive Strength, wet, 6K HTA 5HS 370 gms
  • Compressive Strength, 6K HTA 5HS 370 gms
  • Compressive Strength, wet, 24K IMS WNCF 550 gsm
  • Compressive Strength, 24K IMS WNCF 550 gsm
  • Compressive Strength, 24K IMS UW 200 gsm
  • Compressive Modulus, wet, 6K HTA 5HS 370 gms
  • Compressive Modulus, 6K HTA 5HS 370 gms
  • Compressive Modulus, 24K IMS WNCF 550 gsm
  • Compressive Modulus, wet, 24K IMS WNCF 550 gsm
  • Compressive Modulus, 24K IMS UW 200 gsm
  • Shear Modulus, In-plane, wet, 6K HTA 5HS 370 gms
  • Shear Modulus, In-plane, wet, 24K IMS WNCF 550 gsm
  • Shear Modulus, In-plane, 6K HTA 5HS 370 gms
  • Shear Modulus, In-plane, 24K IMS WNCF 550 gsm
  • Shear Strength, Apparent Interlaminar, wet, 6K HTA 5HS 370 gms
  • Shear Strength, Apparent Interlaminar, 24K IMS WNCF 550 gsm
  • Shear Strength, In-plane, wet, 24K IMS WNCF 550 gsm
  • Shear Strength, In-plane, 24K IMS WNCF 550 gsm
  • Shear Strength, Apparent Interlaminar, 6K HTA 5HS 370 gms
  • Shear Strength, In-plane, wet, 6K HTA 5HS 370 gms
  • Shear Strength, Apparent Interlaminar, 24K IMS UW 200 gsm
  • Shear Strength, In-plane, 6K HTA 5HS 370 gms
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, E' modulus intercept, wet
  • Glass Transition Temp, Tg, peak tan, wet
  • Glass Transition Temp, Tg, E' modulus intercept
  • Glass Transition Temp, Tg, peak tan
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.