MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GY-FR-WRP (ZHS Whitening Red Phosphorus flame retardant, WRP)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • GY-FR-WRP can offer excellent flame retardant effect.
  • Belong to non-halogen flame retardant (no fluorine, chlorine, bromine or other halogen )
  • End products complexes with GY-FR-WRP cause less amount of smoke.
  • GY-FR-WRP can provide excellent decomposition.
  • Can be flame-resistant for a long time (durability)
  • Confer to outstanding tinting ability, can modify the defects of traditional red phosphate flame retardant.
  • Do not cause migration when application
  • Can be well compatible with multi-kinds polymers, resins, plastic, elastomer, electric cable/ wire compounding.
  • GY-FR-WRP with high whiteness offers marvelous color.
Applications:
  • Thermal Setting resin: Phenol, Epoxy, Unsaturated Polyester, Polyester resin , Acrylic resin…etc.
  • Coatings and Various Resins: Flame Retardant paints, all kinds of Acrylic related products, PU, PMMA, Latex, Adhesives
  • Thermal Plastic resin : PVC, PP, Polyolefin, PET, NYLON, POM, PE/EVA, flame retardant electric cable/wire, engineering Plastic….etc.
  • Rubber industry : EPDM, CR, NBR, SBR, SIR, CSM, NR.IIR, various kinds of flame retardant rubber
  • Elastomer: TPE, TPU, SBS, SEBS, TPR, TPV, various kinds of elastomer.
  • Foam Polymers: Applied in multi-kinds of foam products, especially Rigid PU Foam Polymers, EVA foam materials.
  • Others: Printing Ink, paper, furniture plywood, pigment, printing, backing glue, flame retardant master batch, various kinds of flame retardant for electronic products.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Acid Value
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.