Ryton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound with the inherent cost savings of thermoplastics.
Applications: Electric Blanket Thermostat Control, Fry Pan Handles, Hair Dryer Grilles, Motor Brush Holders
Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI Units
Data provided by Chevron Phillips Chemical Company LP.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic