MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify it for high performance service in a wide range of applications. It is mechanically both strong and tough, exhibiting high dielectric strength, and can be used in applications over a broad temperature range. As a fluoropolymer, it is highly resistant to most environmental conditions, including corrosive chemicals and organic solvents, strong acids, alkaline, peroxide and SC1 and SC2 chemistries, and aqueous caustics for handling wet or dry chlorine, bromine, and other halogens.

FEATURES AND BENEFITS

  • Purity- Halar has a very low extractable and leaching levels for the most demanding semiconductor applications.
  • Weldability- Easy to fabricate with conventional welding equipment. Extremely strong welds.
  • Strength- High tensile properties and it is very ductile.
  • Economics- The cost of Halar is easily offset by the expense that would normally be incurred by fire suppression equipment.
  • Fire Safe- Accepted in accordance to FM4910, fire safe materials for clean room construction.
  • Extruded Sheet- Offers the best gauge consistency, surface and tolerances.

Information provided by Compression Polymers Corp - Vycom

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Hardness, Shore D, ASTM D785
  • Tensile Strength, Ultimate, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • CTE, linear, ASTM D696
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Oxygen Index, ASTM D863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CPC - Vycom Co. Compression Plastics Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.