Temper: As Hot Forged - Air Cooled Typical uses: Cu-Ni forgings for sea water exposure Applicable Specifications: Bar – ASTM B151/B151M; Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M; Die – ASTM B283/B283M; Heat Exchanger Tube – ASTM B543/B543M; Pipe – Welded ASTM B467, ASTM B466/B466M, Welded ASTM B608; Plate – ASTM B171/B171M; Rod– ASTM B151/B151M; Rod, Bar & Shapes – ASTM B124/B124M; Sheet, Strip, Roller Bar & Plate – ASTM B122/B122M; Tube – ASTM B359/B359M, ASTM B466/B466M, ASTM B111/B111M, ASTM B395/B395M; Welded ASTM B552 |