Agilus30™ is a Rubber-like PolyJet™ photopolymer family ideal for advanced design verification and rapid prototyping. It produces durable, tear-resistant prototypes that can stand up to repeated flexing and bending. With a Shore A value of 30 in clear, black and white, Agilus30 accurately simulates the look, feel and function of Rubber-like products. 3D print rubber surrounds, overmolds, soft-touch coatings, living hinges, jigs and fixtures, wearables, grips and seals with improved surface texture.Information provided by Stratasys. |