MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Borealis Queo" 0201FX-01 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Queo" 0201FX-01 is an ethylene based octene-1 plastomer, produced in a solution polymerization process using a metallocene catalyst. Queo" 0201FX-01 contains anti block agent, slip agent and stabilizers. CAS-No. 26221-73-8

Typical characteristics:

  • Versatile blending with other polyolefins in film, extrusion and molding applications.
  • Unrivalled sealing and hot tack properties at low temperature
  • Low Coefficient of Friction (C.O.F.) and improved C.O.F. consistency
  • Outstanding toughness
  • Outstanding puncture resistance
  • Low temperature impact strength
  • High clarity
Applications:
  • High speed FFS film
  • Laminated structures requiring very high seal integrity
  • High strength flexible film
  • Sealing layer in coextrusion
Queo 0201FX-01 is intended for use as primary blend partner in high performance seal layers with an additive package designed to offer improved control of the coefficient of friction of coextruded blown films.

Information provided by Borealis AG

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180
  • Dart Drop, ASTM D1709
  • Vicat Softening Point, ISO 306
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 20°
  • Gloss, ASTM D2457, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.