MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NeXolve Thermalbright® C Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: High performance white polyimide film.

Thermalbright® Polyimide is a high performance white polyimide film with wide ranging uses in display applications, electrical insulators, composites, industrial tapes, space structures, and many others. Thermalbright® Polyimide is useful in thermal control applications requiring low absorptivity, high emissivity, UV stability, and high temperature colorfastness.

Thermalbright® Polyimide exhibits high optical density and hiding, making it an excellent high temperature white paint replacement material. In addition to outstanding thermal and optical properties, Thermalbright® Polyimide exhibits the lowest moisture uptake of all commercially available polyimides, at 0.2%.

Thermalbright® Polyimide is available in two grades: Thermalbright® C for Electrostatic Dissipative (ESD) applications, and Thermalbright® N for applications that require electrical insulation. Continuous rolls are available now in 1 mil thickness (25 micron) and in widths up to 60 inches (152 cm).

Information Provided by NeXolve Corporation.

Vendors:
Available Properties
  • Density, ASTM D792-08
  • Water Absorption, ASTM D570-98
  • Tensile Strength, ASTM D882-02
  • Elongation at Break, ASTM D882-02
  • Modulus of Elasticity, ASTM D882-02
  • Volume Resistivity, ASTM D257-91
  • Surface Resistivity per Square, ASTM D257-91
  • CTE, linear, ASTM E831-06
  • Glass Transition Temp, Tg, ASTM E1356-03, DSC
  • Transmission, Visible, ASTM E903-96, Solar Transmittivity
  • Emissivity (0-1), ASTM E408-71, Infrared (Hemispherical)
  • Reflection Coefficient, Visible (0-1), ASTM E903-96, Solar Reflectivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
NeXolve Corporation, Subsidiary of ManTech International Corporation.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.