MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Covestro SOFTCEL® U-1000 Polyol
Categories: Other Engineering Material

Material Notes: Softcel U-1000 Polyol is a low molecular weight polyol.

Properties / Applications: Softcel U-1000 Polyol is a low molecular weight polyol. It may be used with other slabstock performance polyols from Covestro to produce Softcel V foams, which are characterized by their slow recovery and high damping characteristics. Softcel Polyol U-100 is typically used with Ultracel® 3000 (U-3000) polyol or Arcol® HS-100 polymer polyol to produce Softcel V foams. When properly formulated, these foams exhibit slow yet complete recovery from deformation, low resilience, high vibration damping and body conforming characteristics, which may make them useful in a variety of applications, including mattresses and mattress pads, pillows, furniture, wheelchairs, sports equipment, acoustical panels, gasketing and automotive interiors. As with any product, use of Softcel U-1000 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density
  • Viscosity
  • Viscosity
  • Viscosity
  • Flash Point, PMCC
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.