MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route using a proprietary high-energy mixing process which ensures excellent particle distribution and enhances mechanical properties. The key benefits of AMC225xe for structural applications include: weight saving; increased component stiffness; and high fatigue resistance.

The combination of properties achieved with AMC225xe provides the potential for outstanding structural performance in a wide range of markets and applications including:

Motorsport

  • Performance valve train
  • Cylinder liners
  • Pistons
  • Connecting rods
  • Brake callipers
  • Disk Bells
  • Suspension parts
Aerospace & Defense
  • Aero engine vanes
  • Aircraft structure
  • Brakes and Wheels
  • Control Systems
  • Valve Blocks

Information provided by CRP Technology.

Vendors:
Available Properties
  • Density
  • Hardness, Vickers, HV10
  • Tensile Strength, Ultimate, short term exposure
  • Tensile Strength, Ultimate, short term exposure
  • Tensile Strength, Ultimate, short term exposure
  • Tensile Strength, Ultimate, short term exposure
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, short term exposure
  • Tensile Strength, Yield, short term exposure
  • Tensile Strength, Yield, short term exposure
  • Tensile Strength, Yield, short term exposure
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Poissons Ratio
  • Fatigue Strength, R=-1; Kt=1; Rotating Bend
  • Fatigue Strength, R=-1; Kt=1; Rotating Bend
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, Solidus
  • Solidus
  • Processing Temperature, Solution Heat Treatment
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.