MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Hexcel® HexPly® Nature Range NR-M78.1-LT Bio-derived Epoxy Matrix
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® Nature Range NR-M78.1-LT is a formulated, hot melt epoxy resin matrix, especially designed for prepreg applications where short cure cycles using temperatures =110°C are required. Due to its high reactivity, HexPly® Nature Range NR-M78.1-LT can be used for economic, environmentally friendly and fast manufacture of industrial composites. HexPly® Nature Range NR-M78.1-LT is based on a modified, toughened epoxy resin and a highly reactive curative package applicable for pre-impregnation into carbon, glass or aramid fibers, combining the outstanding feature of being curable within e.g. 8 minutes at 120°C and with a shelf life of at least 3 weeks at ambient conditions and at least 7 days at 30°C. NR-M78.1-LT is supplied as low tack resin matrix. The versatility of HexPly® Nature Range NR-M78.1-LT allows a range of processing temperatures, recommended from 110°C up to 160°C. Following a cure cycle in the recommended range, HexPly® Nature Range NR-M78.1-LT demonstrates superior mechanical properties and high glass transition temperatures. The controlled-flow characteristics of HexPly® Nature Range NR-M78.1-LT offers excellent adhesion to auxiliary and core materials like aluminum, wood, thermoplastics and elastomers. The solvent-free, non-corrosive character of HexPly® Nature Range NR-M78.1-LT offsets the commonly known drawbacks of inhouse prepreg systems that typically include hazardous components causing limitations regarding environmental, health and safety conditions.

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Density
  • Viscosity, M78.1-LT @ 5°C/min
  • Viscosity, M78.1-LT @ 5°C/min
  • Viscosity, M78.1-LT @ 5°C/min
  • Glass Transition Temp, Tg, Typical cured, following a 6min cure @130°C
  • Glass Transition Temp, Tg, Optimum cured, following a 15min cure @130°C
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Cure Time, ISO 11357-5, time to 95% conversion
  • Shelf Life
  • Shelf Life
  • Shelf Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.