MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Udel® P-3500 NT LCD PSU
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Udel® P-3500 NT LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.

Polysulfone is a tough, rigid and transparent high-strength thermoplastic that is suitable for long-term use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstands prolonged exposure to high temperatures and repeated sterilization.

Polysulfone is resistant to mineral acids, alkali, salt solutions, detergents and hydrocarbon oils. Contact with polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons should be avoided, as these types of chemical compounds can cause stress cracking or solvate polysulfone resin.

Polysulfone is highly resistant to degradation by gamma or electron beam radiation but can be adversely affected by long term exposure to ultraviolet. Electrical properties of the polymer are very stable over a wide range of temperatures and after immersion in water or exposure to high humidity.

The resin is very safe for food contact uses. It complies with FDA 21 CFR 177, 1655 and may be used in articles intended for repeated use in contact with foods. Additionally, it is approved by the NSF, by the Department of Agriculture for contact with meat and poultry and the 3-A Sanitary Standards of the Dairy Association.

Applications: Appliance Components; Appliances; Automotive Electronics; Dental Applications; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Hospital Goods; Industrial Parts; Medical Devices; Medical/Healthcare Applications; Membranes; Microwave Cookware; Piping; Plumbing Parts; Surgical Instruments; Valves/Valve Parts

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Chemical Resistant; Detergent Resistant; Good Dimensional Stability; Good Sterilizability; Good Surface Finish; Good Toughness; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Tensile Impact Strength, ASTM D1822
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Zone 1, Extrusion
  • Zone 5, Extrusion
  • Melt Temperature, Extrusion
  • Drying Temperature, Extrusion
  • FDA, 21 CFR 177, 1655
  • NSF
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.