Redco™ UHMW polyethylene offers a combination of high impact strength, excellent machinability and low surface friction with outstanding wear and corrosion resistance. FDA, CFIA and USDA compliant Redco™ UHMW reduces material hang ups and enhances material flow; increasing your production and your profits. Standard Color: Natural (white) & Black Typical Applications: Wear strip, channel, diverter arms, bearing blocks, scraper blades, wear rails, star wheels, chute liners, hopper liners, bunk pads, slider blocks, low pressure gears, light duty pulleys, dock fenders/pads, metal detector troughs, trimmer lugs, sprockets, conveyor flights, wear shoes/guides, forklift hose sheaves, skate wheels, rollers, hold down wheels, slides, cutting boards, outrigger pads, etc. Information provided by Redwood Plastics and Rubber |