MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
INEOS Styrolution Styroflex® 2G 66 LE Styrene Butadiene Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styroflex® 2G66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE) suitable for extrusion (blown and cast film) and for injection molding. Styroflex® 2G66 is also used for polymers modification and compatibilization. It is more polar than comparable SBS or SEBS grades and offers a combination of high resilience and toughness with good transparency and process stability. Features: Excellent thermostability, Very high elongation at break, High resilience, High transparency, Regulatory compliant, High flow. Applications: Food packaging and films, Stretch hood/ stretch film, Impact modification / ESCR improvement, Compounding, compatibilization, recycling, Medical devices, Adhesives, Soft touch injection molding; toys, 2-K inj. mold.

Information provided by Styrolution.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Oxygen Transmission Rate, 0% RH
  • Melt Flow, ISO 1133, Volumetric; cm3/10 min
  • Hardness, Shore A, ISO 868
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Vicat Softening Point, ASTM D 1525, B/2 120C/H
  • Refractive Index, ISO 489, Sodium D Line
  • Haze, ASTM D 1003
  • Transmission, Visible, ASTM D1003
  • Melt Temperature, ISO 294
  • Mold Temperature, ISO 294
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.