MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) (extended Stress-Strain Tabular Data)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792, DAM
  • Density, ISO 1183, DAM
  • Filler Content, DAM
  • Linear Mold Shrinkage, Transverse; DAM
  • Linear Mold Shrinkage, Transverse; DAM
  • Linear Mold Shrinkage, Flow, ISO 294-4, DAM
  • Linear Mold Shrinkage, Flow, Flow; DAM
  • Linear Mold Shrinkage, Flow, Flow; DAM
  • Hardness, Rockwell M, ASTM D785, DAM
  • Hardness, Rockwell R, ASTM D785, DAM
  • Tensile Strength at Break, ISO 527, 50%RH
  • Tensile Strength at Break, ISO 527, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, 50%RH
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Strength, ASTM D638, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Tensile Stress at Strain, ISO 11403-1/-2, DAM
  • Tensile Stress at Strain, ISO 11403-1/-2, 50%RH
  • Elongation at Break, ISO 527, DAM
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ISO 527, 50%RH
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ASTM D638, 50%RH
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ASTM D638, DAM
  • Elongation at Break, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, 50%RH
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ASTM D638, DAM
  • Tensile Modulus, ISO 527, 50%RH
  • Tensile Modulus, ISO 527, DAM
  • Flexural Strength, ASTM D790, 50%RH
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Strength, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, 50%RH
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Flexural Modulus, ASTM D790, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Compressive Strength, ASTM D695, DAM
  • Shear Strength, ASTM D732, 50%RH
  • Shear Strength, ASTM D732, DAM
  • Izod Impact, Notched, ASTM D256, 50%RH
  • Izod Impact, Notched, ASTM D256, DAM
  • Izod Impact, Notched, ASTM D256, DAM
  • Izod Impact, Notched, ASTM D256, 50%RH
  • Izod Impact, Unnotched, ASTM D4812, 50%RH
  • Izod Impact, Unnotched, ASTM D4812, DAM
  • Izod Impact, Unnotched (ISO), ISO 180/1U, DAM
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 50%RH
  • Charpy Impact Unnotched, ISO 179/1eU, 50%RH
  • Charpy Impact Unnotched, ISO 179/1eU, DAM
  • Charpy Impact Unnotched, ISO 179/1eU, 50%RH
  • Charpy Impact Unnotched, ISO 179/1eU, DAM
  • Charpy Impact, Notched, ISO 179/1eA, 50%RH
  • Charpy Impact, Notched, ISO 179/1eA, DAM
  • Charpy Impact, Notched, ISO 179/1eA, DAM
  • Charpy Impact, Notched, ISO 179/1eA, 50%RH
  • Tensile Creep Modulus, 1 hour, ISO 899, 50%RH
  • Tensile Creep Modulus, 1000 hours, ISO 899, 50%RH
  • Volume Resistivity, ASTM D257, DAM
  • Volume Resistivity, IEC 60093, DAM
  • Surface Resistance, ASTM D257, DAM
  • Surface Resistance, IEC 60093, 50%RH
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Constant, ASTM D150, DAM
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dielectric Strength, ASTM D149, DAM; Short Time
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Dissipation Factor, ASTM D150, DAM
  • Comparative Tracking Index, IEC 60112, DAM
  • Comparative Tracking Index, UL 746A, DAM
  • Comparative Tracking Index, ASTM D3638, DAM
  • CTE, linear, Parallel to Flow, ASTM E 831, DAM
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Parallel to Flow, ASTM E 831, DAM
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Parallel to Flow, ASTM E 831, DAM
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Parallel to Flow, ASTM E 831, DAM
  • CTE, linear, Transverse to Flow, ASTM E 831, DAM
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Transverse to Flow, ASTM E 831, DAM
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Transverse to Flow, ASTM E 831, DAM
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
  • CTE, linear, Transverse to Flow, ASTM E 831, DAM
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
  • Melting Point, ISO 11357-1/-3, 10°C/min, First Heat; DAM
  • Melting Point, ASTM D3418, DAM
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, DAM
  • UL RTI, Electrical, UL 746B, DAM
  • UL RTI, Electrical, UL 746B, DAM
  • UL RTI, Electrical, UL 746B, DAM
  • UL RTI, Mechanical with Impact, UL 746B, DAM
  • UL RTI, Mechanical with Impact, UL 746B, DAM
  • UL RTI, Mechanical with Impact, UL 746B, DAM
  • UL RTI, Mechanical without Impact, UL 746B, DAM
  • UL RTI, Mechanical without Impact, UL 746B, DAM
  • UL RTI, Mechanical without Impact, UL 746B, DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flammability, UL94, IEC 60695-11-10, DAM
  • Flammability, UL94, UL94, DAM
  • Flammability, UL94, UL94, DAM
  • Flammability, UL94, UL94, DAM
  • Oxygen Index, ASTM D2863, DAM
  • Oxygen Index, ISO 4589-1/-2, DAM
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Melt Temperature, DAM; Optimum
  • Melt Temperature, DAM
  • Mold Temperature, DAM; optimum
  • Mold Temperature, DAM
  • Drying Temperature, DAM
  • Dry Time, DAM
  • Moisture Content, DAM
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.