MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NRI Viper-Skin™ Carbon Fiber Composite
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Polyurethane, TS

Material Notes: Viper-Skin™ is the first bi-axial, hybrid carbon and glass fiber polyurethane pre-impregnated system that blends the unsurpassed strength and stiffness of carbon with the ease and use of a moisture-cured, factory-saturated fiber.

Typical Applications:

  • Transmission and distribution pipelines
  • Oil and gas risers
  • Mechanical dents and defects
  • Girth welds on vessels and pipelines
  • Process piping: chemicals, oil, gases, water and steam
Benefits:
  • Moisture-cured polyurethane resin reduces composite preparation time by over 50%
  • Factory-saturation optimizes fiber to resin ration and provides a material with a constant strength property
  • Non-shielding
  • Can be applied to damp, sweating, or immersed surfaces
  • No heating or post-curing required
  • Can be applied to any geometry including, but not limited to elbows, Tees, and flanges
  • Design conforms to ASME PCC-2, ASME B31, ISO TS24817, DOT, API, and CSA Z662 standards for nonmetallic reinforcing solutions

Information provided by NRI® Innovative Composite Solutions

Vendors:
Available Properties
  • Thickness, Laminate
  • Hardness, Shore D
  • Flexural Strength
  • Poissons Ratio
  • Shear Strength, In-plane
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Set time
  • Cure Time, Set time
  • Cure Time, Set time
  • Cure Time, Set time
  • Cure Time, Set time
  • Pot Life
  • Working Life
  • Working Life
  • Working Life
  • Working Life
  • Working Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.