Available Properties |
---|
- Density, ISO 1183
- Viscosity, ASTM D3835
- Melt Flow, ASTM D1238
- Hardness, Shore A, ISO 868, Injection Molded
- Hardness, Shore A, ISO 868, Injection Molded
- Hardness, Shore A, ISO 868, Injection Molded
- Hardness, Shore A, ISO 888, Change in Air, 1000 hr
- Hardness, Shore A, ISO 888, Change in Air, 168 hr
- Hardness, Shore A, ISO 888, Change in Air, 1000 hr
- Hardness, Shore A, ISO 888, Change in Air, 168 hr
- Hardness, Shore A, ISO 888, Change in Air, 1008 hr
- Hardness, Shore A, ISO 888, Change in Air, 168 hr
- Hardness, Shore A, ISO 888, Change in Air, 1000 hr
- Hardness, Shore A, ISO 888, Change in Air, 1008 hr
- Hardness, Shore A, ISO 888, Change in Air, 1008 hr
- Tensile Strength at Break, ISO 37, Flow, Type 1, 20 in/min
- Tensile Strength at Break, ISO 37, Across Flow, Type 1, 20 in/min
- Tensile Strength at Break, ISO 188, Flow, Type 1, Change in Air
- Tensile Strength at Break, ISO 188, Flow, Type 1, Change in Air
- Tensile Strength at Break, ISO 188, Flow, Type 1, Change in Air
- Tensile Strength at Break, ISO 188, Across Flow, Type 1, Change in Air
- Tensile Strength at Break, ISO 188, Across Flow, Type 1, Change in Air
- Tensile Strength at Break, ISO 188, Across Flow, Type 1, Change in Air
- Tensile Stress at Strain, ISO 37, Across Flow, Type 1, 20 in/min
- Tensile Stress at Strain, ISO 37, Flow, Type 1, 20 in/min
- Tensile Stress at Strain, ISO 188, Across Flow, Type 1, Change in Air, 168 hr
- Tensile Stress at Strain, ISO 188, Across Flow, Type 1, Change in Air, 1000 hr
- Tensile Stress at Strain, ISO 188, Across Flow, Type 1, Change in Air, 1008 hr
- Tensile Stress at Strain, ISO 188, Flow, Type 1, Change in Air, 1008 hr
- Tensile Stress at Strain, ISO 188, Flow, Type 1, Change in Air, 168 hr
- Tensile Stress at Strain, ISO 188, Flow, Type 1, Change in Air, 1000 hr
- Elongation at Break, ISO 37, Flow, Type 1, 20 in/min
- Elongation at Break, ISO 37, Across Flow, Type 1, 20 in/min
- Elongation at Break, ISO 188, Flow, Type 1, Change in Air
- Elongation at Break, ISO 188, Flow, Type 1, Change in Air
- Elongation at Break, ISO 188, Across Flow, Type 1, Change in Air
- Elongation at Break, ISO 188, Across Flow, Type 1, Change in Air
- Elongation at Break, ISO 188, Flow, Type 1, Change in Air
- Elongation at Break, ISO 188, Across Flow, Type 1, Change in Air
- Tear Strength Test, ISO 34-1, Flow
- Tear Strength Test, ISO 34-1, Across Flow
- Tear Strength, ISO 34-1, Across Flow, Method Ba, Angle (Unnicked), 20 in/min
- Tear Strength, ISO 34-1, Flow, Method Ba, Angle (Unnicked), 20 in/min
- Taber Abrasion, mg/1000 Cycles, SAE J948, 1000 G, CS-10 Wheel
- Compression Set, ISO 815, Type 1
- Compression Set, ISO 815, Type 1
- Compression Set, ISO 815, Type 1
- Processing Temperature, Melt, Injection
- Rear Barrel Temperature, Injection
- Middle Barrel Temperature, Injection
- Front Barrel Temperature, Injection
- Nozzle Temperature, Injection
- Zone 1, Extrusion
- Zone 2, Extrusion
- Zone 3, Extrusion
- Zone 4, Extrusion
- Zone 5, Extrusion
- Die Temperature, Extrusion
- Mold Temperature, Injection
- Injection Pressure, Injection
- Back Pressure, Injection
- Cushion, Injection
- Screw Speed, Extrusion
- Screw Speed, Injection
|
| | |