MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Xydar® G-930 LCP, 30% glass fiber
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: 30% glass fiber, general purpose for injection molding

Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.

The moldability of this resin is exceptional. Xydar® G-930 can fill very thin walls over long flow lengths with little or no flash, even at mold temperatures below 200°F (93°C). In addition, it has low warpage in molded products and exceptional weld line strength.

This material exhibits high strength and stiffness (even at elevated temperatures), low coefficient of thermal expansion, high deflection temperature, inherent flame resistance, and outstanding resistance to most chemicals, weathering, and radiation.

-Black: G-930 BK
-Natural: G-930 NT

Markets/Uses: Automotive Bobbins; Engine Sensors; Header Connector; Lead Frames

Applications: Automotive Applications; Automotive Electronics; Bobbins; Electrical Parts; Electrical/Electronic Applications; Industrial Applications; Industrial Parts

Features: Chemical Resistant; Flame Retardant; Good Moldability; Good Weather Resistance; High Stiffness; High Strength; Low Warpage; Radiation (Gamma) Resistant

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, ASTM D3638
  • CTE, linear, Parallel to Flow, ASTM D696
  • CTE, linear, Transverse to Flow, ASTM D696
  • Hot Ball Pressure Test, IEC 60695-10-2, Pass
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2/B, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • UL RTI, Mechanical without Impact
  • Flammability, UL94
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Clamp Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.