EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial and pressure pipe , gas pipe, drinking water pipe, relining , fittings. Information provided by Iran Petrochemical Commercial Co. |