MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik TEGOMER® DA 100 N Dispersant
Categories: Other Engineering Material

Material Notes: Product description: TEGOMER® DA 100 N is a polymeric dispersant technology which can be applied for the dispersion of solid particles in hydrophobic media.

Application:

  • TEGOMER® DA 100 N is used as dispersant in liquid pastes for the dispersion and stabilization of organic pigments and fillers.
  • TEGOMER® DA 100 N can be applied in mineral and vegetable oil for the dispersion of solid particles coming from the filler and pigment range, nanoparticles or also solid additive ingredients, e.g. antioxidants, flame retardants and others. Those pastes or colorants are used for polyolefines or styrenic thermoplastic systems.
  • TEGOMER® DA 100 N is a suitable dispersant for the manufacture of pigment dispersion in phthalates and adipates which are intended to be used for PVC application.
  • TEGOMER® DA 100 N has a good compatibility in 100 % systems based on acrylates, hydrophobic polyether polyols or polyester polyols whereas hydrophilic polyether polyols are not compatible with it.
Benefits: TEGOMER® DA 100 N is a liquid dispersant applicable in a wide range of hydrophobic phases. It allows the manufacture of thermoplastic and duroplastic materials with efficient color strength development due to high pigment stability and dispersion degree. Pastes based on TEGOMER® DA 100 N are long term stable since this polymeric dispersant allows even in low viscous media to avoid settlement. TEGOMER® DA 100 N allows higher loading of pigments and nanomaterials in hydrophobic media.

Information provided by Evonik

Vendors:
Available Properties
  • Density
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.