Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&D Center. Polypropylene copolymer adhesive resin Lushan PR298 is used as adhesive layer between epoxy powder layer and PP compound top coats layer. Polypropylene copolymer adhesive resin Lushan PR298 been exported to many countries all over the world, and successfully applied to wrapped coated or direct coated 3PP buried anti-corrosion steel pipe and coated steel plastic composite pipe for exploration and transportation of natural gas, oil, chemical liquids, water, etc.Information provided by Lushan |