MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Redwood Plastics Redco™ CG-SS80 Sheet Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Commercial Grade silicone sheeting is designed to be used in applications where physical properties are not critical but extreme temperature resistance and reliable performance are still needed. Silicone rubber has the combined properties of resilience, high temperature stability, and general inertness unavailable in any other elastomer. Silicones are generally unaffected by extended exposure to temperatures from -75º up to +232ºF and are also resistant to aging and degradation from sunlight and ozone. Silicone is a polysiloxane chain. Unlike other rubbers, its molecular matrix does not contain carbon, but consists of silicone and oxygen atoms. It can be formulated to achieve flame resistance, electrical or thermal conductivity, electrostatic dissipative (ESD) as well as FDA and medical compliance.

Typical Applications:

  • High temp seal and gaskets
  • Wipers & squeegees
  • Electrical Insulators
  • FDA approved applications
  • Digital print roller covers
  • O-rings
Core Advantages:
  • Exceptional high & low temperature resistance
  • Unaffected by ozone, weather and UV radiation
  • Good electrical insulator
  • Self-extinguishable
  • Maintains a stable shore hardness and consistant physical properties through wide temperature range

Information provided by Redwood Plastics and Rubber

Vendors:
Available Properties
  • Hardness, Shore A, ASTM D 2240
  • Hardness, Shore A, ASTM D 1056, Accelerated Aging @ 30% RH
  • Tensile Strength, ASTM D 412
  • Tensile Strength, ASTM D 1056, Accelerated Aging @ 30% RH
  • Elongation at Break, ASTM D412
  • Elongation at Break, ASTM D 1056, Accelerated Aging @ 30% RH
  • Compression Set, ASTM D 395 Method B
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.