MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Selenis SELEKT XP 310 PCTG Copolyester for Injection Molding
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: Selenis Selekt XP 310 is a copolyester that is suitable for injection molding applications. From thin wall and intricate parts to thicker cross-sections where toughness is required. Injection molded parts made from Selenis Selekt XP 310 are water-clear and glossy, whilst virtually unbreakable. Selenis Selekt XP 310 features excellent impact strength and outstanding chemical resistance. Fast injection cycles are possible due to high flowability. Thanks to Selenis Selekt XP 310 high dimensional stability, multiple parts products may be assembled with snap-fit connectors, maintaining the strength required to sustain daily wear and tear. Molded parts maybe sterilized by Gamma-radiation or EtO sterilization process.

Information provided by Selenis.

Vendors:
Available Properties
  • Bulk Density
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Viscosity Test, ISO 1628-5, Intrinsic
  • Linear Mold Shrinkage, ASTM D 955
  • ASTM Color, ASTM D6290, b*
  • ASTM Color, ASTM D6290, L*
  • Tensile Strength, ISO 527 -1/- 2, (σm)
  • Tensile Strength, Yield, ISO 527 -1/- 2, (σy)
  • Elongation at Break, ISO 527 -1/- 2, Nominal, (εtb)
  • Elongation at Yield, ISO 527 -1/- 2, (εm)
  • Elongation at Yield, ISO 527 -1/- 2, (εy)
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Notched (ISO), ISO 180/A, 50% RH
  • Izod Impact, Unnotched (ISO), ISO 180/U
  • Izod Impact, Unnotched (ISO), ISO 180/U
  • Izod Impact, Unnotched (ISO), ISO 180/U, 50% RH
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact Unnotched, ISO 179-1/1eU, 50% RH
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Charpy Impact, Notched, ISO 179-1/1eA, 50% RH
  • Puncture Energy, ISO 6603-2/3.3 m/s, Impact Behavior, Energy Maximum Load
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306/A50
  • Glass Transition Temp, Tg, ASTM D3418
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 60ยบ
  • Yellow Index, ASTM (E313-73)
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • Transmission, Visible, Disk
  • UV Transmittance, Disk
  • UV Transmittance, Disk
  • UV Transmittance, Disk
  • UV Transmittance, Disk
  • UV Transmittance, Disk
  • Melt Temperature
  • Drying Temperature, to avoid chips sticking together in dryer hopper
  • Drying Temperature
  • Moisture Content, dried
  • Dew Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.