Temper: As Continuous Cast Casting Characteristics: High – Fluidity; Medium – Effect of Section Size, Casting Yield; Med-High – Gassing; Low - Drossing, Shrinkage in Solidification Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding Typical uses: Bells; Bearings; Bushings; Piston Rings; Valve Bodies |